Product name: CuZn10

Main alloying elements: copper (Cu), zinc (Zn)


Mechanical properties:

Tensile strength: 280 - 320 MPa (megapascals)

Yield strength: 120 - 180 MPa

Elongation at break: 40 - 50%

Hardness (Rockwell): -

Modulus of elasticity: 100 - 110GPa


Physical Properties:

Density: 8.4 g/cm³

Melting point: approx. 900 - 940 °C

Thermal conductivity: 120 - 140 W/(m K)

Electrical conductivity: 27 - 35% IACS (International Annealed Copper Standard)


Chemical composition (in percent by weight):

Copper (Cu): approx. 90 - 91%

Zinc (Zn): approx. 9 - 10%


Heat treatment:

After casting, CuZn10 can be strengthened by various heat treatments, such as annealing or work hardening.


Corrosion resistance:

CuZn10 offers good resistance to corrosion in most atmospheric conditions as well as in fresh water. However, it can be susceptible to corrosion in saline or acidic environments.


Applications:

CuZn10 is used in a variety of applications including:

Plumbing and heating systems: piping, fittings

Electrical engineering: connectors, contacts

Jewelry making: jewelry parts

General mechanical engineering: screw connections, housing


Please note that the values given are indicative and may vary slightly depending on the manufacturing process and specific batch. It is recommended to always check the manufacturer's exact specifications.