Alloy 1.4016 technical data sheet:
General information:
Alloy: 1.4016
Trade names: X6Cr17, AISI 430
Material number: 1.4016
DIN standard: X6Cr17
UNS number: S43000
Chemical composition:
Carbon content (C): 0.08% max.
Silicon content (Si): 1.00% max.
Manganese (Mn): 1.00% max.
Phosphorus (P): 0.04% max.
Sulfur (S): 0.03% max.
Chromium (Cr): 16.00 - 18.00%
Physical Properties:
Density: 7.70 g/cm³
Melting point: 1425 - 1510 °C
Thermal conductivity: 25 W/(m*K)
Electrical conductivity: 0.60 Ωmm²/m
Specific electrical resistance: 0.17 μΩm
Mechanical properties:
Tensile strength: 450 - 600 N/mm²
Yield point: 250 - 350 N/mm²
Elongation at break: 20 - 28%
Hardness: 180 - 230 HB
Heat treatment:
Hardenability: by tempering at temperatures between 950 and 1050 °C
Tempering hardness: at 600 - 700 °C for an optimal combination of hardness and toughness
Application areas:
Kitchen and sanitary industry (e.g. cutlery, kitchen appliances, sinks)
Automotive industry (e.g. exhaust systems, catalytic converters)
General EngineeringArchitecture (e.g. facade cladding, railings)
Please note that the values given here are guide values and may vary depending on the manufacturing process, dimensions and testing method. It is recommended to check the manufacturer's specifications before use.