Alloy 1.4028 technical data sheet:
General information:
Alloy: 1.4028
Trade names: X30Cr13, AISI 420B
Material number: 1.4028
DIN standard: X30Cr13
UNS number: S42020
Chemical composition:
Carbon content (C): 0.26 - 0.35%
Silicon content (Si): 1.00% max.
Manganese (Mn): 1.50% max.
Phosphorus (P): 0.04% max.
Sulfur (S): 0.03% max.
Chromium (Cr): 12.50 - 14.50%
Physical Properties:
Density: 7.7 g/cm³
Melting point: 1450 - 1510 °C
Thermal conductivity: 30 W/(m*K)
Electrical conductivity: 0.25Ωmm²/m
Specific electrical resistance: 0.40 μΩm
Mechanical properties:
Tensile strength: 700 - 1000 N/mm²
Yield point: 450 - 800 N/mm²
Elongation at break: 8 - 18%
Hardness: 200 - 260 HB
Heat treatment:
Hardenability: by tempering at temperatures between 950 and 1050 °C
Tempering hardness: at 200 - 650 °C for an optimal combination of hardness and toughness
Application areas:
Cutting tools, surgical instruments and injection molds
Valves, pump parts and fittings in the chemical industry
Components in the aerospace industry
Blades, screws and shafts in the food industry
Please note that the values given here are guide values and may vary depending on the manufacturing process, dimensions and testing method. It is recommended to check the manufacturer's specifications before use.